ASTM E350-18
- standard by ASTM International, 03/15/2018
- Standard Test Methods for Chemical Analysis of Carbon Steel, Low-Alloy Steel, Silicon Electrical Steel, Ingot Iron, and Wrought Iron
- Category: ASTM
$88.00
$44.00
Full Description
1.1 These test methods cover the chemical analysis of carbon steels, low-alloy steels, silicon electrical steels, ingot iron, and wrought iron having chemical compositions within the following limits:
Element | Composition Range, % |
Aluminum | 0.001 to 1.50 |
Antimony | 0.002 to 0.03 |
Arsenic | 0.0005 to 0.10 |
Bismuth | 0.005 to 0.50 |
Boron | 0.0005 to 0.02 |
Calcium | 0.0005 to 0.01 |
Cerium | 0.005 to 0.50 |
Chromium | 0.005 to 3.99 |
Cobalt | 0.01 to 0.30 |
Columbium (Niobium) | 0.002 to 0.20 |
Copper | 0.005 to 1.50 |
Lanthanum | 0.001 to 0.30 |
Lead | 0.001 to 0.50 |
Manganese | 0.01 to 2.50 |
Molybdenum | 0.002 to 1.50 |
Nickel | 0.005 to 5.00 |
Nitrogen | 0.0005 to 0.04 |
Oxygen | 0.0001 to 0.03 |
Phosphorus | 0.001 to 0.25 |
Selenium | 0.001 to 0.50 |
Silicon | 0.001 to 5.00 |
Sulfur | 0.001 to 0.60 |
Tin | 0.002 to 0.10 |
Titanium | 0.002 to 0.60 |
Tungsten | 0.005 to 0.10 |
Vanadium | 0.005 to 0.50 |
Zirconium | 0.005 to 0.15 |
1.2 The test methods in this standard are contained in the sections indicated as follows:
| Sections |
|
|
Aluminum, Total, by the 8-Quinolinol Gravimetric Product Details
Document History ASTM E350-18ASTM E350-12ASTM E350-95(2005)e1ASTM E350-95(2005)ASTM E350-95(2000)e1ASTM A300-68Standard Specification for Notch Toughness Requirements for Normalized Steel Plates for Pressure Ves.. $27.00 $54.00 |